Injection Molds: Easier Decisions in Mold Design Using Virtual Molding

Upfront simulation of the core pins’ deformation helps choose the mold materials

Bild 1 – Simulativer Vergleich der Deformation von Kernen aus Wolframcarbid (links) und aus 1.4034 (rechts) am Ende des Einspritzens – Unter konstanten Prozessbedingungen ist der Kern aus dem Material mit niedrigerem E-Modul am Ende des Füllens um das Dreifache verformt. / Figure 1 – Simulative comparison of the deformation of core pins made of tungsten carbide (left) and 420 stainless steel (right) at the end of the filling of the cavity – the material with the lower modulus of elasticity deforms three times more under constant process conditions.
Bild 1 – Simulativer Vergleich der Deformation von Kernen aus Wolframcarbid (links) und aus 1.4034 (rechts) am Ende des Einspritzens – Unter konstanten Prozessbedingungen ist der Kern aus dem Material mit niedrigerem E-Modul am Ende des Füllens um das Dreifache verformt. / Figure 1 – Simulative comparison of the deformation of core pins made of tungsten carbide (left) and 420 stainless steel (right) at the end of the filling of the cavity – the material with the lower modulus of elasticity deforms three times more under constant process conditions.
Bild 2 – Darstellung des Schmelzedrucks in zwei Kavitäten mit Kernen aus Wolframcarbid (links), bzw. aus 1.4034  (rechts) – Der obere Bildausschnitt zeigt den Füllstand, bei dem sich das Ungleichgewicht des Schmelzeflusses zum ersten Mal zeigen lässt. Am Ende der Füllphase (im unteren Bildausschnitt) sieht man diese eindeutig. / Figure 2 – Demonstration of the melt pressure in two cavities with core pins made of tungsten carbide (left) and 420 stainless steel (right) – The upper section shows the point in filling where the imbalance is visible for the first time. At the end of filling (lower section) this phenomena can be seen clearly.
Bild 2 – Darstellung des Schmelzedrucks in zwei Kavitäten mit Kernen aus Wolframcarbid (links), bzw. aus 1.4034 (rechts) – Der obere Bildausschnitt zeigt den Füllstand, bei dem sich das Ungleichgewicht des Schmelzeflusses zum ersten Mal zeigen lässt. Am Ende der Füllphase (im unteren Bildausschnitt) sieht man diese eindeutig. / Figure 2 – Demonstration of the melt pressure in two cavities with core pins made of tungsten carbide (left) and 420 stainless steel (right) – The upper section shows the point in filling where the imbalance is visible for the first time. At the end of filling (lower section) this phenomena can be seen clearly.
Bild 2 – Darstellung des Schmelzedrucks in zwei Kavitäten mit Kernen aus Wolframcarbid (links), bzw. aus 1.4034  (rechts) – Der obere Bildausschnitt zeigt den Füllstand, bei dem sich das Ungleichgewicht des Schmelzeflusses zum ersten Mal zeigen lässt. Am Ende der Füllphase (im unteren Bildausschnitt) sieht man diese eindeutig. / Figure 2 – Demonstration of the melt pressure in two cavities with core pins made of tungsten carbide (left) and 420 stainless steel (right) – The upper section shows the point in filling where the imbalance is visible for the first time. At the end of filling (lower section) this phenomena can be seen clearly.
Bild 2 – Darstellung des Schmelzedrucks in zwei Kavitäten mit Kernen aus Wolframcarbid (links), bzw. aus 1.4034 (rechts) – Der obere Bildausschnitt zeigt den Füllstand, bei dem sich das Ungleichgewicht des Schmelzeflusses zum ersten Mal zeigen lässt. Am Ende der Füllphase (im unteren Bildausschnitt) sieht man diese eindeutig. / Figure 2 – Demonstration of the melt pressure in two cavities with core pins made of tungsten carbide (left) and 420 stainless steel (right) – The upper section shows the point in filling where the imbalance is visible for the first time. At the end of filling (lower section) this phenomena can be seen clearly.

SIGMASOFT® provides a variety of methods to forecast the shrinkage and warpage of plastic parts. Along with this, one can also simulate the deformation of inserts or core pins during filling. SIGMA simulates and compares the deformation of core pins made of two different mold materials under equal process conditions. The calculations are based on the imbalanced melt flow inside the cavity and the mechanical properties of the two materials.

There are many questions that injection mold manufacturers confront daily regarding the variety of mold materials which are available in the market. What type of steel should be used for which part of the mold? Whether it is the thermal conductivity of the steel used for the cavity insert, the diameter of a suitable ejector pin or even the mechanical stability of the core pins, SIGMASOFT® Virtual Molding leads to the correct decision.

In SIGMASOFT® every mold material, e.g. steel, isolation, etc., is taken into account with its thermal and mechanical properties. As an example, one can simulate the heating up phase or the developement of hotspots during several injection cycles having the thermal conductivity and specific heat capacity of all the mold materials. Besides the prediction of shrinkage and warpage of plastic parts, SIGMASOFT® also simulates the deformation of inserts and core pins during filling. These calculations are based on possible imbalances in the filling of the cavity and of course the mechanical properties of the steel.

SIGMA Plastic Services, Inc. (IL), the American subsidiary of SIGMA Engineering GmbH, simulated an interesting project in cooperation with two companies, CAVAFORM (FL) and Crafts Technology (IL). In the project the deformation of core pins made of different materials during filling of the cavity was evaluated. The investigation was done for an injection mold with 16 cavities, which is used to produce centrifuge tubes. In 8 of these cavities, core pins made of tungsten carbide are integrated to form the inside of the tubes. 420 stainless steel is used for the other 8 core pins. Simulative analysis of the filling phase shows an imbalance, which comes to existence after about 85% of filling has passed and becomes more obvious near the end of filling (Figure 2). This imbalance is caused by the asymmetrical geometry of the screw in the cap area of the tube and leads to a force, which tends to deform the core pins during the filling of the cavity. Due to the lower module of elasticity of 420 stainless steel, pins made of this steel are deformed about 3 times more compared to the pins made of tungsten carbide (Figure 1).

The described case is just an example of the many details of an injection mold, which can get misplanned during the mold design phase. SIGMASOFT® Virtual Molding provides even the most experienced mold manufacturers with a detailed insight of the injection molding process. With a very low effort and based only on the thermophysical and mechanical phenomena, even before ordering the mold units, they can examine and evaluate the effect of changes in the mold. Thus, simulation provides a sound basis for decisions and supports the mold design from the beginning.



SIGMA Engineering GmbH
52072 Aachen
Germany


Better informed: With YEARBOOK, NEWSLETTER, NEWSFLASH and EXPERT DIRECTORY

Stay up to date and subscribe to our monthly eMail-NEWSLETTER and our NEWSFLASH. Get additional information about what is happening in the world of cleanrooms with our printed YEARBOOK. And find out who the cleanroom EXPERTS are with our directory.

Systec & Solutions GmbH PMS Ecolab PPS